Galvanizing is one of the most widespread anti-corrosion treatments in the metalworking sector, but it is not a technique applicable indiscriminately to any part or material. Each type — hot-dip galvanizing, cold galvanizing, electrolytic galvanizing — requires specific surface preparation, and the results in terms of aesthetics and protection vary much more than one might think. Let’s look at how to orient yourself in detail.
A necessary premise: galvanizing is not our core business, as we do not perform galvanizing ourselves. However, the contribution that Trebi can make to the galvanizing process could be very significant. Want to know why? Then… happy reading!
At TREBI, we design, manufacture, and install robotic machines that work mainly on brass, aluminum, cast iron, and steel components intended for faucets, orthopedic components, foundry castings, and mechanically machined parts — materials and productions that, as we will see later, in most cases do not undergo galvanizing or only do so in specific cases.
The cost of hot-dip, cold, or electrolytic galvanizing.
This article therefore stems from a technical in-depth study on the subject, not from direct experience as suppliers of metal finishing services (galvanizing plants). That said, the principles of robotic surface preparation that we deal with every day — deburring, grinding, finishing — naturally apply to this field as well, and for this reason, we wanted to explore it further. If you are wondering: what is the cost of hot-dip galvanizing per kg? What is the cost of cold galvanizing per kg? You will not find a specific answer in this article, but you will be able to understand some key aspects that, if correctly interpreted and applied to the hot-dip galvanizing process and similar, could still save you considerably. How? With our robotic metal finishing machines! Have you ever heard, for example, of Trebi’s renowned grinding robots?
Hot-dip galvanizing: characteristics
In hot-dip galvanizing, metal components are immersed in tanks of molten zinc at approximately 450°C. Upon contact with the metal, the zinc reacts with the iron to form a zinc-iron intermetallic alloy that integrates structurally with the part, rather than just coating it like a simple surface film. This is why hot-dip galvanizing offers corrosion and abrasion resistance that is difficult to match with other treatments: a surface scratch does not expose the underlying metal to atmospheric agents as would happen with conventional painting.
Hot-dip galvanizing is the treatment typically used on metalwork parts — structures, railings, gates, welded elements made in small series or custom-made — where resistance in outdoor environments is the priority. Hot-dip galvanizing is the treatment of choice for steel components (pipes and fittings) intended for plumbing, a field in which hot-dip galvanizing demonstrates all its aptitudes for protecting metal in particularly stressful applications.
Cold galvanizing
Cold galvanizing is, in fact, a coating based on synthetic resins containing zinc. It offers a thinner protective layer compared to hot-dip galvanizing and requires more frequent maintenance. It is typically applied to mechanically machined steel parts (turning or milling operations).
Electrolytic (galvanic) galvanizing
This involves immersing the part in an electrolytic solution containing zinc salts: the passage of current deposits a thin layer of zinc (5-30 μm) on the surface. It is the preferred technique for components with welds or heat treatments that could be compromised by the high temperatures of hot-dip galvanizing (zinc melts at 420°C).
Which materials can be galvanized (and which cannot)
Hot-dip or cold galvanizing is not suitable for every metal. It is mainly recommended for steel and iron, which react well with molten zinc to form a stable, adherent coating. Cast iron can also be galvanized, but it requires special technical precautions to avoid defects related to its porosity.
The situation is different for other metals widely used in mechanical processing: copper, brass, and bronze have poor zinc adhesion, which is why in industrial practice they are almost never galvanized. Stainless steel, being already inherently resistant to corrosion, does not need this treatment. Finally, aluminum can only be galvanized electrolytically and only on specific alloys — not with the hot-dip process.
Surface preparation: a different phase for each hot-dip or cold galvanizing technique for iron and steel.
Here lies the heart of the process, and it is also the most misunderstood point. Each type of galvanizing requires a different preparation, both chemical and mechanical.
Hot-dip galvanizing: degreasing, pickling, fluxing — and a rough grinding upstream
The standard chemical cycle includes:
1. Degreasing — hot alkaline or acid bath to remove residual processing oils and greases
2. Pickling — immersion in dilute hydrochloric acid to eliminate rust and mill scale
3. Washing — rinsing in water to eliminate acid residues
4. Fluxing — immersion in a zinc and ammonium chloride solution, which protects the surface from oxidation until the moment of immersion and improves the iron-zinc reaction
5. Preheating — heating to 110-120°C to reduce thermal shock
6. Immersion in the molten zinc bath at 440-450°C
Before all this, however, the part must arrive clean for hot-dip galvanizing: no coarse burrs, evident welding slag, or marked processing residues. This is where a rough grinding phase comes into play, necessary to prevent these defects from compromising the pickling and, consequently, the adhesion of the zinc. It is not a fine or aesthetic process — the standard (UNI EN ISO 1461) does not require a uniform aesthetic finish: small roughness or color differences are tolerated, while flux residues, harmful lumps, or uncoated areas are not — but it is a rough mechanical preparation aimed at removing what the chemical bath alone cannot handle. This operation, traditionally manual, can today be robotized, with advantages in terms of repeatability and consistency of the result batch after batch.
When galvanizing is mandatory: what the standards really say
No standard says “in this sector you must galvanize”. Galvanizing becomes mandatory in two ways: when it is written in a binding document (contract, specifications, project specification) or when it is part of the product itself defined by a standard.
Let’s look at the cases.
1. When protection is imposed by the project or specifications: UNI EN 1090-2 and UNI EN ISO 14713
For steel structures with CE marking, UNI EN 1090-2 (Chapter 10 and Annex F) requires that the anti-corrosion protection system be defined in the execution specifications. It depends on the environment and the expected service life. The standard doesn’t tell you to “galvanize”: it tells you that you must choose and specify. If you write hot-dip galvanizing in the project or specifications, from that moment it is mandatory and must be performed according to UNI EN ISO 1461.
To make a sensible choice, you need UNI EN ISO 14713. It doesn’t impose anything; it’s a guide. Part 1 starts from the corrosivity category of the environment (from C1 to CX, ISO 9223) and the duration you want to achieve. From there, you understand if galvanizing is enough or if a duplex system (zinc plus paint) is needed. Part 2 concerns hot-dip galvanizing and explains how to design the part so that it turns out well.
This often happens in structural metalwork, infrastructure, construction and outdoor structures, industrial plants, parapets, and walkways.
2. When galvanizing is already within the product standard
In some products, galvanizing is part of the definition. If you buy or produce that product, galvanizing is necessarily present:
- Hot-dip galvanized bolts: UNI EN ISO 10684.
- Tubes with zinc coating applied in automatic plants: UNI EN 10240.
- Continuously galvanized sheets: UNI EN 10346.
Elements for electrical lines and systems (for example, poles): in many cases, the manufacturer declares galvanizing according to UNI EN ISO 1461 or, upon request, according to CEI 7-6.
For these products, UNI EN ISO 1461 often does not apply because specific standards apply. Always check which standard your specifications refer to.
Sectors where galvanizing must meet certain quality criteria
When hot-dip galvanizing is required “according to standard”, the benchmark is UNI EN ISO 1461. This happens in steel structures with CE marking (with UNI EN 1090-2), in infrastructure, in metalwork intended for outdoors, and in industrial plants. The criteria are as follows:
Thickness: minimums depend on the thickness of the steel. In the 2009 edition, for steels over 6 mm, they are 70 µm local and 85 µm average. Between 3 and 6 mm, they are 55 and 70 µm; between 1.5 and 3 mm, they are 45 and 55 µm; under 1.5 mm, they are 35 and 45 µm. For cast irons from 6 mm up, they are 70 and 80 µm; under 6 mm, they are 60 and 70 µm. The standard was revised in 2022, so check the values in the current edition.
Surface appearance: flux residues are not allowed, nor are zinc lumps and ashes when they compromise the use of the part. Small color differences or wet storage stains are not grounds for rejection if the thickness remains above the minimum.
Coating continuity: no uncovered areas or defects that compromise protection.
Uncoated areas: these are repaired, but with precise limits. Each area cannot exceed 10 cm² and the total cannot exceed 0.5% of the surface. Repair is done with sprayed zinc or zinc-rich paint. Beyond those limits, the part is re-galvanized.
In structures with CE marking, UNI EN 1090-2 adds other obligations: measures against acid penetration into weld cracks, vent and drainage holes for closed spaces, and attention to the risk of liquid metal embrittlement, which also depends on the class of the zinc bath (Annex F). The galvanizer also issues the declaration of conformity to UNI EN ISO 1461.
Quality does not depend only on the zinc bath!
What I often see: “badly” galvanized parts where the problem is not the galvanizer. A welding slag, a burr, a processing residue, or a surface irregularity are enough to create defects. Pickling does not remove them, so the zinc adheres poorly or accumulates irregularly. For this reason, UNI EN ISO 14713-2 and UNI EN 1090-2 assign the manufacturer the task of preparing the part. The quality of the coating also depends on what you do before the bath.
The TREBI point of view: upstream mechanical preparation.
This is where our trade meets galvanizing. We do not galvanize parts, but we remove what compromises galvanizing: burrs, welding slag, irregularities. Grinding and removal of imperfections in many metalwork shops are still done by hand, with results that change from operator to operator and from batch to batch. A robotic system works with constant parameters (pressure, speed, abrasive) on every part. The result is repeatable, the process is under control, and the surface entering the galvanizing process is consistent. If your specifications require the criteria of UNI EN ISO 1461, arriving at the bath with a uniformly prepared part is already half the job.
Cold galvanizing: surface preparation is absolutely essential
Here the situation changes radically. Being a true coating, cold galvanizing faithfully replicates the texture of the underlying part: every roughness, every trace of processing visible before application will remain visible even after. The required preparation is therefore more similar to that of a normal quality coating:
- Removal of mill scale (if present)
- Complete degreasing
On mechanically machined parts, this preparation phase is normally performed by tumbling: the parts are loaded into a vibrating tank together with abrasive stones, which in their movement eliminate burrs and uniform the surface. It is an effective process, but with known limits — long cycle times, less control over complex geometries or parts with delicate surfaces, and a result that is not always consistent from batch to batch.
This same preparation can also be achieved with robotic systems designed and produced by Trebi, which apply constant processing parameters (pressure, speed, type of abrasive) on every single part, guaranteeing a more uniform and predictable result compared to tumbling — a significant advantage, given that here the starting finish is visible in the final result.
Electrolytic galvanizing: same principle as cold galvanizing
Also in the case of electrolytic galvanizing, since the deposited layer is very thin (5-30 μm), the finish of the starting part directly affects the final aesthetic result. Pre-treatment includes pre-degreasing, pickling, and a second degreasing before immersion in the electrolytic bath.
TREBI’s experience in robotic preparation
Whether it is the rough grinding pre-hot-dip galvanizing or the finer preparation required before cold galvanizing or before electrolytic galvanizing — the latter typically entrusted to tumbling — the processing/preparation phases can be effectively robotized, with a concrete gain in terms of repeatability, defined cycle times, and constant quality on large volumes, which manual processing or traditional tumbling struggle to guarantee uniformly. More quality and certain, convenient cost definition.
We deal with robotic cells for deburring and metal finishing, with experience on metalwork components, foundry castings (aluminum, cast iron, brass), and mechanically machined steel parts.
If you work with productions that involve a galvanizing treatment and want to evaluate how to automate the surface preparation phase — upstream of the chemical bath or coating — contact us: we can analyze your production cycle. Together we can develop a plan to propose robotic solutions of undoubted advantage.